Hobart Welding Products H-10 GUN, 180 manual Conditions That Affect Weld Bead Shape

Page 38

9-4. Conditions That Affect Weld Bead Shape

NOTE

Weld bead shape depends on gun angle, direction of travel, electrode extension (stickout), travel speed, thickness of base metal, wire feed speed (weld current), and voltage.

 

10°

 

Push

 

10°

Perpendicular

Drag

GUN ANGLES AND WELD BEAD PROFILES

Short

Normal

Long

 

ELECTRODE EXTENSIONS (STICKOUT)

 

 

 

 

Short

Normal

Long

FILLET WELD ELECTODE EXTENSIONS (STICKOUT)

Slow

Normal

Fast

 

GUN TRAVEL SPEED

S-0634

 

 

OM-925 Page 34

Image 38
Contents Processes DescriptionFrom Hobart to You Table of Contents − Parts List Arc Welding Hazards Symbol UsageMarks a special safety message Electric Shock can killFlying Metal can injure eyes ARC Rays can burn eyes and skinWelding can cause fire or explosion Buildup of GAS can injure or killCalifornia Proposition 65 Warnings About Pacemakers Principal Safety StandardsEMF Information LES Décharges Électriques peuvent être mortelles Signification des symboles− Consignes DE Sécurité − À Lire Avant Utilisation LES Fumées ET LES GAZ peuvent être dangereuxLES Pièces Chaudes peuvent cau- ser des brûlures graves LE Soudage peut causer un incen- die ou une explosionLES Particules Projetées peu- vent blesser les yeux LE Bruit peut affecter l’ouïe’EMPLOI Excessif peut Faire Risque D’INCENDIE OU D’EXPLOLA Chute DE L’APPAREIL peut blesser LES Pièces Mobiles peuvent cau- ser des blessuresConsignes relatives aux stimulateurs cardiaques Principales normes de sécuritéInformation sur les champs électromagnétiques Specifications − SpecificationsSymbols And Definitions − DefinitionsOutput Duty Cycle % Duty Cycle And OverheatingAmperes VAC Model Output AmperesAmperage Volt-Ampere CurvesVoltage Installing Work Clamp − InstallationInstalling Welding Gun Process/Polarity Table Changing PolarityInstalling Gas Supply Special installation may be SectionDo not move or operate unit where it could tip Electrical Service Guide For 230 VAC Model Installing Wire Spool And Adjusting Hub TensionThreading Welding Wire Hold wire tightly to keep it From unraveling− Operation ControlsWeld Parameter Chart For 115 VAC Model 217 618-A Weld Parameter Chart For 230 VAC Model 217 754-B Overload Protection − Maintenance &TROUBLESHOOTINGRoutine Maintenance Drive Motor ProtectionReplacing Gun Contact Tip Changing Drive Roll Or Wire Inlet GuideTurn Off power before replacing contact tip To Reassemble Gun Cleaning Or Replacing Gun LinerDisconnect gun from unit Replacing Switch And/Or Head Tube Does not run Troubleshooting TableTrouble Remedy − Electrical Diagram Circuit Diagram For 115 VAC ModelCircuit Diagram For 230 VAC Model − MIG Welding Gmaw Guidelines Typical MIG Process ConnectionsThickness to Amperage a Typical MIG Process Control SettingsWire Size Amperage Range Select VoltageHolding And Positioning Welding Gun Conditions That Affect Weld Bead Shape Gun Movement During Welding Poor Weld Bead CharacteristicsGood Weld Bead Characteristics Troubleshooting − Excessive Penetration Troubleshooting − Excessive SpatterTroubleshooting − Porosity Possible Causes Corrective ActionsTroubleshooting − Burn-Through Troubleshooting − Lack Of PenetrationTroubleshooting − Incomplete Fusion Troubleshooting − Waviness Of Bead Troubleshooting − DistortionCommon MIG Shielding Gases Troubleshooting Guide For Semiautomatic Welding EquipmentWire does not feed ApplicationWelding arc not stable Wire slipping in drive rolls OM-925 − Parts List Main AssemblyDia Part Description Quantity Dia Part Description Quantity Mkgs H-10 Gun 195Optional Drive Rolls OptionsService SupportContact your Distributor for Hobart Welding Products