MISADJUSTMENTS(S)

COURSE OF ACTION

 

 

 

 

 

 

STICK WELDING PROBLEMS

 

Stick electrode “Blasts Off” when arc

1.

Weld current may be set too

 

is struck.

 

high for electrode size. Reduce

 

 

 

 

current control setting, or use a

 

 

 

 

larger diameter electrode.

 

 

 

 

 

Stick electrode “sticks” in the weld

1.

The weld current may be set too

Contact your Local Lincoln Authorized

puddle.

 

low. Increase the current control

Field Service Facility for technical

 

 

 

setting or use a smaller diame-

troubleshooting assistance.

 

 

 

ter electrode.

 

 

 

 

 

 

 

 

 

 

 

CAUTION

If for any reason you do not understand the test procedures or are unable to perform the tests/repairs safely, contact your Local Lincoln Authorized Field Service Facility for technical troubleshooting assistance before you proceed.

SQUARE WAVE TIG 175 PRO

Page 25
Image 25
Lincoln Electric TIG 175 PRO manual Symptoms Misadjustmentss Course of Action, Field Service Facility for technical