PROTECTIVE GAS

Both argon and helium work when welding aluminum. Argon is preferred, due to its lower cost and consump- tion rate. This gas also tends to stabilize the arc, thus making it easy to operate. For some applications, however, the use of helium, or argon-helium blends, is recommended due to better weld penetration and faster travel speed. Helium is especially suitable for welding thick workpieces. The recommended gas flow rates are shown in table 5.

 

TABLE 5

 

 

 

Current (A)

 

Helium cfh-(l/min)

50

 

29 - (14)

100

 

29 - (14)

150

 

42 - (20)

200

 

42 - (20)

250

 

53 - (25)

300

 

53 - (25)

 

 

 

AC TIG WELDING QUICK START UP

WARNING

ELECTRIC SHOCK can kill.

Have an electrician install and service this equipment.

Turn the input power off at the fuse box, dis- connect or unplug supply lines and allow machine to sit for five minutes minimum to allow the power capacitors to discharge before working inside this equipment.

Do not touch electrically hot parts.

------------------------------------------------------------------------

Connect the shielding gas – typically argon – using a appropriate regulator. Connect the foot amptrol, torch and work lead to the power source.

With the work cable connected to a properly grounded work piece, turn the power source on.

The Invertec V205 T AC/DC TIG is ready to AC TIG weld with the following features:

AC TIG

Trigger Mode in 2 step mode

Local control

Pulser off

AC Square Wave

AC Balance 65% EN

AC Frequency 100HZ

Pre Flow .5sec.

Post Flow 5 sec.

High Freq Start

Change from Local to Remote control by pushing front panel push button.

Set the maximum output current desired using the Output Control. Initiate the arc by closing the arc start switch. The Amptrol will control the output current from 10 amps to current level set by Output Control.

To change the AC Frequency, press and hold the Parameter button for 3 seconds. The AC Frequency is now selected and can be varied by the Output Control. The frequency is displayed on the digital meter. After about 5 seconds, the power source will switch back to the welding mode ready to weld with the new selected AC Frequency.

To change the AC Balance, press and hold the Parameter button for 3 seconds, AC Frequency is selected, press the Parameter button again and AC Balance is selected. Adjust the Output Control for the desired AC Balance. After about 5 seconds, the power source will switch back to the welding mode ready to weld with the new selected AC Balance.

To change the Post Flow time, repeatedly push the Parameter button until the Post Flow indicator light is on. Adjust the Output control to the desired Post Flow time as indicated on digital display.