B-10

LEARNING TO WELD

B-10

 

 

 

FIGURE B.12

Penetration

Unless a weld penetrates close to 100% of the metal thickness, a butt weld will be weaker than the material welded together. In the example shown in Figure B.13, the total weld is only half the thickness of the material thus the weld is only approximately half as strong as the metal.

45°

FIGURE B.15

Welding In The Vertical Position

Welding in the vertical position can be done either ver- tical-up or vertical-down. Vertical-up is used whenever

alarger, stronger weld is desired. Vertical-down is used primarily on sheet metal 5/32” (3.9 mm) and under for fast, low penetrating welds.

FIGURE B.13

FIGURE B.14

In the example shown in Figure B.14, the joint has been welded so that 100% penetration could be achieved. The weld, if properly made, is as strong as or stronger than the original metal.

Fillet Welds

When welding fillet welds, it is very important to hold the wire electrode at a 45° angle between the two sides or the metal will not distribute itself evenly. The gun nozzle is generally formed at an angle to facilitate this. See Figure B.15.

WARNING

Use of this unit on thicker materials than recom- mended may result in poor welds. The welds may “look” good, but may just be “sitting” on top, of the plate. This is called “Cold Casting” and will result in weld failure.

Vertical-up And Overhead Welding

The problem, when welding vertical-up, is to put the molten metal where it is wanted and make it stay there. If too much molten metal is deposited, gravity will pull it downwards and make it “drip”. Therefore, a certain technique has to be followed.

When welding out-of-position, run stringer beads. Don’t whip, break the arc, move out of the puddle, or move too fast in any direction. Use Wire Feed Speed (WFS) in the low portion of the range. The general technique and proper gun angle is illustrated in Figure B.16.

Generally, keep the electrode nearly perpendicular to the joint as illustrated. The maximum angle above per- pendicular may be required if porosity becomes a problem.

WELD-PAK 3200HD

Image 24
Contents WELD-PAK 3200HD Safety California Proposition 65 WarningsElectric Shock can kill Welding Sparks can cause fire or explosion IiiPrécautions DE Sûreté Sûreté Pour Soudage a L’ArcThank You Please Examine Carton and Equipment For Damage ImmediatelyMaster Table of Contents for ALL Sections Installation Technical Specifications WELD-PAK 3200HDSafety Precautions Identify and Locate ComponentsElectric Shock can kill Work Clamp Installation Select Suitable LocationOutput Connections StackingGUN Installation Work Cable InstallationConnecting Gun Cable to the WELD-PAK GAS ConnectionFigure A.5 Input Connections Code Requirements for Input ConnectionsRequirements For Rated Output Undercarriage Assembly Figure A.7 WELD-PAK 3200HDDesign Features OperationGeneral Description Recommended ProcessesControls and Settings Welding CapabilityLimitations Wire Loading Welding OperationsSequence of Operation Friction Brake Adjustment Wire ThreadingCleaning Tip And Nozzle Process GuidelinesMaking a Weld Changing Machine Over to Feed Other Wire Sizes Welding with Gmaw MIGOverload Protection Learning to Weld Learning to WeldARC-WELDING Circuit SELF-SHIELDED Fcaw Welding ARCGmaw MIG Welding ARC Process SelectionCommon Metals Joint Types and PositionsFor Gmaw MIG Process For Fcaw Innershield ProcessWelding In The Vertical Position PenetrationFillet Welds Machine SET UP for the SELF-SHIELDED Fcaw Process Welding Techniques for the SELF- Shielded Fcaw ProcessVertical-down Welding Correct Welding PositionCorrect Electrical Stickout ESO Correct Welding SpeedHelpful Hints PracticeMachine SET UP for the Gmaw MIG Process Welding Techniques for the Gmaw MIG ProcessFor the WELD-PAK 3200HD, use the following Troubleshooting Welds To Eliminate a Ropy Convex Bead in order of importanceTo Correct Poor Penetration in order of impor- tance To Eliminate Stubbing* in order of importanceProper Gun Handling Application Chart Accessories Optional AccessoriesK586-1 Deluxe Adjustable Gas Regulator Hose Kit Replacement Parts Maintenance Maintenance Safety PrecautionsRoutine Maintenance GUN and Cable Maintenance Configuration of Components in Wire Feeding SystemFor Magnum 100L GUN Contact Tip Cable Liner Drive RollComponent Replacement Procedures Changing the Contact TIPChanging Drive Roll Changing Liner GUN Handle PartsLiner trim length Troubleshooting HOW to USE Troubleshooting GuideProblems Possible Areas Symptoms Misadjustments Recommended Course of ActionContact your local Lincoln Authorized Field Service FacilityWelding Problems Diagrams WELD-PAK 3200HD Wiring DiagramWELD-PAK 3200HD How To Read Shop Drawings New Lessons in Arc WeldingNeed Welding Training? $700.00Precaucion Warnung