Hobart Welding Products 230 manual Common MIG Shielding Gases, Application

Page 43

6-16. Common MIG Shielding Gases

This is a general chart for common gases and where they are used. Many different combinations (mixtures) of shielding gases have been developed over the years. The most commonly used shielding gases are listed in the following table.

 

 

Application

 

 

 

 

 

 

Gas

Spray Arc Steel

Short Circuiting Steel

Short Circuiting

Aluminum

 

Stainless Steel

 

 

 

 

 

 

 

 

 

Argon

 

 

 

X

 

 

 

 

 

Argon + 25% CO2

 

X

 

 

 

 

 

 

 

80% or greater Argon +

X

X1

 

 

balance CO2 or Oxygen

 

 

 

 

 

 

100% CO2

 

X

 

 

 

 

 

 

 

Tri-Mix2

 

 

X

 

1Limited short circuiting use

290% HE + 7-1/2% AR + 2-1/2% CO2

6-17. Troubleshooting Guide For Semiautomatic Welding Equipment

Problem

Probable Cause

Remedy

 

 

 

Wire feed motor operates, but

Too little pressure on wire feed rolls.

Increase pressure setting on wire feed rolls.

wire does not feed.

 

 

Incorrect wire feed rolls.

Check size stamped on wire feed rolls, replace to match

 

 

 

wire size and type if necessary.

 

 

 

 

Wire spool brake pressure too high.

Decrease brake pressure on wire spool.

 

 

 

 

Restriction in the gun and/or assembly.

Check and replace cable, gun, and contact tip if

 

 

damaged. Check size of contact tip and cable liner,

 

 

replace if necessary.

 

 

 

Wire curling up in front of the

Too much pressure on wire feed rolls.

Decrease pressure setting on wire feed rolls.

wire feed rolls (bird nesting).

 

 

Incorrect cable liner or gun contact tip size.

Check size of contact tip and check cable liner length

 

 

 

and diameter, replace if necessary.

 

 

 

 

Gun end not inserted into drive housing properly.

Loosen gun securing bolt in drive housing and push gun

 

 

end into housing just enough so it does not touch wire

 

 

feed rolls.

 

 

 

 

Dirty or damaged (kinked) liner.

Replace liner.

 

 

 

Wire feeds, but no gas flows.

Gas cylinder empty.

Replace empty gas cylinder.

 

 

 

 

Gas nozzle plugged.

Clean or replace gas nozzle.

 

 

 

 

Gas cylinder valve not open or flowmeter not adjusted.

Open gas valve at cylinder and adjust flow rate.

 

 

 

 

Restriction in gas line.

Check gas hose between flowmeter and wire feeder, and

 

 

gas hose in gun and cable assembly.

 

 

 

 

Loose or broken wires to gas solenoid.

Have Factory Authorized Service Agent repair wiring.

 

 

 

 

Gas solenoid valve not operating.

Have Factory Authorized Service Agent replace gas

 

 

solenoid valve.

 

 

 

 

Incorrect primary voltage connected to welding power

Check primary voltage and relink welding power source

 

source.

for correct voltage.

 

 

 

OM-235 281 Page 39

Image 43
Contents File MIG Gmaw OM-235 281AProcesses DescriptionProtect Your Investment From Hobart to YouTable of Contents Warranty HOT Parts can burn Symbol UsageArc Welding Hazards Electric Shock can killFlying Metal or Dirt can injure eyes Fumes and Gases can be hazardousARC Rays can burn eyes and skin Welding can cause fire or explosionMoving Parts can injure Welding Wire can injureFire or Explosion hazard Falling Equipment can injureAbout Implanted Medical Devices Principal Safety StandardsCalifornia Proposition 65 Warnings EMF InformationUNE Décharge Électrique peut entraîner la mort Symboles utilisésLES Fumées ET LES GAZ peuvent être dangereux DES Pièces Chaudes peuvent provoquer des brûlures gravesLE Soudage peut provoquer un in cendie ou une explosion LA Chute DE L’APPAREIL peut blesser LE Bruit peut endommager l’ouïeLES Bouteilles peuvent exploser si elles sont endommagées Risque D’INCENDIE OU D’EXPLO- SionLES Fils DE Soudage peuvent provoquer des blessures Proposition californienne 65 AvertissementsLE Soudage À L’ARC risque de provoquer des interférences Information EMF Principales normes de sécuritéEn ce qui concerne les implants médicaux OM-235 281 Welding Power Source Duty Cycle And Overheating SpecificationsOverheating 40.0 35.0 30.0 25.0 20.0 15.0 10.0 100 150 200 250 300 Volt-Ampere CurvesVoltage AmperageMIG GUN Installing Welding GunInstalling Work Clamp Connecting To Weld Output TerminalsElectrode Negative Dcen Setting Gun Polarity For Wire TypeInstalling 2 lb Wire Spool And Adjusting Hub Tension Changing PolarityInstalling 33 lb Wire Spool And Adjusting Hub Tension Installing 10 lb Wire Spool And Adjusting Hub TensionRear Panel Installing Gas SupplyTools Needed 1-1/8, 5/8 Positioning Jumper Links Turn off and disconnect input powerInput Amperes At Rated Output Electrical Service GuideHz Single Input VoltageConductors from unit Selecting a Location And Connecting Input PowerDo not move or operate unit where it could tip Special installation may beThreading Welding Wire Turn Off unit, and disconnect input power Controls Wire Speed Control3070 2080 1090 Weld Parameters Selecting Wire, Gas and Control SettingsBefore maintaining Routine MaintenanceDisconnect power Supplementary ProtectorsTurn Off power Replacing Drive Roll And Wire Inlet GuideRemoving Knob From Front Panel Turn Off power before replacing contact tip Aligning Drive Rolls and Wire GuideReplacing Gun Contact Tip Turn Off power before Installing cable hangers Installing Cable HangersCable Hanger Screws Tools Needed Turn off welding power source/wire feeder Welding Trouble Remedy Welding Troubleshooting TableWire Drive/Gun Troubleshooting Table Wire Drive/Gun Trouble RemedyTypical MIG Process Connections − MIG Welding Gmaw GuidelinesSelect Voltage Typical MIG Process Control SettingsWire Size Amperage Range AmperageGroove Welds Holding And Positioning Welding GunShort Normal Long Conditions That Affect Weld Bead ShapePush Perpendicular DragGood Weld Bead Characteristics Poor Weld Bead CharacteristicsGun Movement During Welding Possible Causes Corrective Actions Troubleshooting − Excessive SpatterTroubleshooting − Porosity Troubleshooting − Excessive PenetrationTroubleshooting − Incomplete Fusion Troubleshooting − Lack Of PenetrationTroubleshooting − Burn-Through Direction Troubleshooting − Waviness Of BeadTroubleshooting − Distortion Base metal to moveCommon MIG Shielding Gases Troubleshooting Guide For Semiautomatic Welding EquipmentApplication Drive rolls if necessary Welding arc not stable Wire slipping in drive rollsReadjust welding parameters Welding power source− Electrical Diagram 10 − Fig 17 − Fig Main AssemblyItem Dia Part Description Quantity Mkgs Center Baffle w/Components Center Baffle w/Components -1Item Rear Panel w/Components Front Panel w/Components 234 Wire Drive Assembly Wire Drive Assembly237 H200L4−15 GunKnurl Drive Roll For Hard Shell Cored Wires AccessoriesSupport ServiceAssistance Hobart Welding Products Contact your Distributor for