Table
| Type of Imperfection |
| Imperfections Not Allowed |
|
|
|
|
|
|
IBM 14" TFT, XGA (OmniBook 4150†/4150B, “IBM74E”,
Electrical Imperfections:
Bright dots (a)
Dark dots (a)
Mechanical Imperfections:
Polarizer scratches (d) Polarizer dents, bubbles (e)
∙4 or more single bright dots (2 or more in central area:
∙8 or more single dark dots.
∙3 or more double bright dots.
∙4 or more double dark dots.
∙9 or more total bright and dark dots.
∙2 or more triple dark dots.
∙Any occurrence of 2 bright dots within 15 mm.
∙Any occurrence of 2 dark dots within 5 mm.
∙4 or more scratches
∙4 or more dents or bubbles
∙Any scratch over 5 mm long and 0.01 mm wide, or over 0.1 mm wide.
∙Any dent or bubble over 0.4 mm avg. dia.
IBM 14" TFT, XGA (OmniBook 4100/4150†, “IBM74”,
Electrical Imperfections:
Bright dots (a)
Dark dots (a)
∙8 or more single bright dots.
∙8 or more single dark dots.
∙9 or more total bright and dark dots.
∙Any occurrence of double bright dots.
∙3 or more double dark dots.
∙Any occurrence of triple bright dots (or triple dark dots).
∙Any occurrence of 2 bright or dark dots within 20 mm.
LG 14" TFT, XGA (OmniBook 4100/4150†)
Electrical Imperfections:
Bright dots (a)
Dark dots (a)
Mechanical Imperfections:
Spots (b)
Lines (c)
Polarizer scratches (d) Polarizer dents, bubbles (e)
∙7 or more single bright dots.
∙7 or more single dark dots.
∙3 or more double bright dots.
∙3 or more double dark dots.
∙11 or more total bright and dark dot imperfections.
∙Any occurrence of triple bright dots (or triple dark dots).
∙Any occurrence of 3 bright dots within 20 mm (or 3 dark dots).
∙6 or more spots
∙4 or more lines
∙5 or more scratches
∙9 or more dents or bubbles
∙Any spot over 0.5 mm avg. dia.
∙Any line over 3 mm long and 0.07 mm wide, or over 0.1 mm wide.
∙Any scratch over 20 mm long and 0.02 mm wide, or over 0.05 mm wide.
∙Any dent or bubble over 0.5 mm avg. dia.
HP OmniBook 4100/4150 | Reference Information |