Lincoln Electric IM546 manual 6OPERATION, Changing Machine Over to Feed Other Wire Sizes

Page 20

B-6OPERATION

thinner, CO2 gas is recommended because it gives equal or better performance than a blended gas at a lower cost. A mixed gas consisting of 75 to 80% Argon and 20 to 25% CO2 is recommended for welding on heavier gauge [12 gauge (2,5 mm) for example] steel.

The WELD-PAK 100 is suitable for .035" aluminum wire and .030" stainless wire. Refer to Table B.1 for recommended procedure settings.

 

 

Shielding

Voltage/Wire Speed

Process

Welding Wire

Gas

16 ga

14 ga

12 ga

10 ga

MIG DC+

.035 Dia

100% Argon

B-5

D-7

D-9

D-9

 

4043 Aluminum

 

 

 

 

 

 

Wire

 

 

 

 

 

MIG DC+

.035 Dia

100% Argon

B-5

C-7

D-9

D-10

 

5356 Aluminum

 

 

 

 

 

 

Wire

 

 

 

 

 

 

 

 

 

 

 

 

MIG DC+

.030 Dia

98% Argon/

A-3

C-6

D-7.5

D-7.5

 

308L Stainless

2% Oxygen

 

 

 

 

 

Steel Wire

 

 

 

 

 

 

 

 

 

 

 

 

TABLE B.1

CHANGING MACHINE OVER TO FEED OTHER WIRE SIZES

The WELD-PAK 100 is shipped from the factory ready to feed 0.035” (0,9 mm) diameter wire. To operate the WELD-PAK 100 with other sizes of wire, it is neces- sary to change the contact tip and change the drive roll over to other sizes. Refer to Changing the Contact Tip and Changing the Drive Roll, in the MAINTE- NANCE section, for specific information on these pro- cedures.

WELDING WITH GMAW (MIG)

Shielding Gas

When using the GMAW process, obtain and install the K610-1 MIG Conversion Kit and a cylinder of carbon dioxide (CO2) or argon-carbon dioxide mixed shielding gas. Refer to the ACCESSORIES section for more information about installing the K610-1 Kit for use with the WELD-PAK 100.

1.For CO2, open the cylinder very slowly. For argon- mixed gas, open cylinder valve slowly a fraction of a turn. When the cylinder pressure gauge pointer

WELD-PAK 100

stops moving, open the valve fully.

2.If using a regulator with an adjustable flow meter, close the gun trigger and adjust the flow to give 15

20 cubic ft per hour (CFH) (7 – 10 I/min) [use 20

25 CFH (10 – 12 I/min) when welding out of

position or in a drafty location for CO2]. For argon mixed gas, trigger to release gas pressure, and turn off the adjust the flow to give 25 – 30 CFH (12 – 14 I/min).

3.Keep the cylinder valve closed, except when using the WELD-PAK 100. When finished welding:

a) Close the cylinder valve to stop gas flow.

b) Depress the gun trigger briefly to release the pressure in the gas hose.

c) Turn off the WELD-PAK 100.

OVERLOAD PROTECTION

Output Overload

The WELD-PAK 100 is equipped with a circuit breaker and a thermostat which protects the machine from damage if maximum output is exceeded. The circuit breaker button will extend out when tripped. The cir- cuit breaker must be manually reset.

Thermal Protection

The WELD-PAK 100 has a rated output duty cycle of 20%. If the duty cycle is exceeded, a thermal protector will shut off the output until the machine cools to a rea- sonable operating temperature. This is an automatic function of the WELD-PAK 100 and does not require user intervention. The fan continues to run during cooling.

Electronic Wire Drive Motor Protection

The WELD-PAK 100 has built-in protection for wire drive motor overload.

Image 20
Contents Safety Depends on You WELD-PAK 100 PlusSafety ARC Welding can be hazardousCylinder may explode if damaged Electric and Magnetic Fields IiiPrécautions DE Sûreté Sûreté Pour Soudage a LʼArcPlease Examine Carton and Equipment For Damage Immediately Master Table of Contents for ALL Sections Vii INSTALLATIONA-1 Technical Specifications WELD-PAKIdentify and Locate Components 2INSTALLATIONSafety Precautions INSTALLATIONA-3 Select Suitable LocationOutput Connections Stacking4INSTALLATION GUN InstallationWork Cable Installation Connecting Gun Cable to the WELD-PAKINSTALLATIONA-5 Figure A.56INSTALLATION Input ConnectionsRequirements For Rated Output Code Requirements for Input ConnectionsObserve all safety information throughout this manual OPERATIONB-1Fumes and Gases can be dangerous Welding Sparks can cause fire or explosion2OPERATION Wire Loading OPERATIONB-3Welding Operations Sequence of Operation4OPERATION Friction Brake AdjustmentWire Threading Cleaning Tip And Nozzle OPERATIONB-5Process Guidelines Making a WeldChanging Machine Over to Feed Other Wire Sizes 6OPERATIONWelding with Gmaw MIG Overload ProtectionLearning to Weld Learning to WeldARC-WELDING Circuit SELF-SHIELDED Fcaw Welding ARCFor Gmaw MIG Process Gmaw MIG Welding ARCProcess Selection Machine SET UP for the SELF-SHIELDED Fcaw Process Common MetalsWelding Techniques for the SELF- Shielded Fcaw Process For Fcaw Innershield ProcessCorrect Electrical Stickout ESO Correct Welding SpeedElectrode Voltage Setting Wire Feed Speed oo Helpful HintsPractice Back-SteppingMachine SET UP for the Gmaw MIG Process Welding Techniques for the Gmaw MIG ProcessElectrode Voltage Setting Wire Feed Speed ooMild Steel Joint Types and Positions PenetrationButt Welds Fillet WeldsWelding In The Vertical Position Vertical-down WeldingTroubleshooting Welds To Eliminate a Ropy Convex Bead in order of importanceTo Correct Poor Penetration in order of impor- tance To Eliminate Stubbing* in order of importanceProper Gun Handling Application Chart MIG Conversion ACCESSORIESC-1Optional Accessories 2NOTES Routine Maintenance MAINTENANCED-1Maintenance Safety Precautions 2MAINTENANCE GUN and Cable MaintenanceComponent Replacement Procedures For Magnum 100L GUNMAINTENANCED-3 Changing Drive RollLiner trim length 4MAINTENANCEChanging Liner MAINTENANCED-5 GUN Handle Parts6NOTES TROUBLESHOOTINGE-1 HOW to USE Troubleshooting Guide2TROUBLESHOOTING Troubleshooting GuideProblems Possible Areas Symptoms Misadjustments Recommended Course of ActionTROUBLESHOOTINGE-3 Feeding Problems4TROUBLESHOOTING Welding Problems100 Wiring DiagramsWeldpak 100 Wiring Diagram 2NOTES WELD-PAK PartsMain Exploded Diagram 2PARTSDescription Reqʼd Complete Drive ASSEMBLY/MOTOR 4PARTSCase Front Assembly PARTS5RECTIFIER, FAN and Bracket Assembly 6PARTSCenter Panel Assembly PARTS7Magnum 100L Assembly 8PARTSSquare Wave TIG Square Wave TIG How To Read Shop Drawings New Lessons in Arc WeldingNeed Welding Training? $700.00Precaucion Guards off Superseded