2-3. Welding Gun Duty Cycle And Overheating

CAUTION

WELDING LONGER THAN RATED DUTY CYCLE can damage gun and void warranty.

Do not weld at rated load longer than shown below.

 

Using gasless flux cored wire reduces gun duty cycle.

warn7.1 8/93

Definition

0

10

Minutes

Duty Cycle is percentage of 10 minutes that gun can weld at rated load without overheating.

.023 To .045 in (0.6 To 1.1 mm)

Hard Or Flux Cored Wires

100% Duty Cycle At 200 Amperes

Using CO2

100% Duty Cycle At 150 Amperes

Using Mixed Gases

Continuous Welding

.023 To .045 in (0.6 To 1.1 mm) Hard Or Flux Cored Wires

60% Duty Cycle At 300 Amperes

Using CO2

60% Duty Cycle At 200 Amperes

Using Mixed Gases

6 Minutes Welding

4 Minutes Resting

 

SB1.1 8/93

2-4. Volt-Ampere Curves

VOLTS

35

30

25

20

15

10

5

0

0

100

200

300

400

AMPERES

1 Normal Volt-Ampere Curves

The volt-ampere curves show the

1normal minimum and maximum voltage and amperage output capa- bilities of the welding power source. Curves of other settings fall be- tween the curves shown.

ssb1.1 10/91 – 196 844 / S-0700

OM-198 683 Page 10

Page 14
Image 14
Hobart Welding Products OM-198 683C manual Welding Gun Duty Cycle And Overheating, Volt-Ampere Curves, Definition