11-5. Positioning Electrode Holder
10°-30°
90°90°
End View of Work Angle | Side View of Electrode Angle |
GROOVE WELDS | |
45° | |
| |
45° |
|
End View of Work Angle | Side View of Electrode Angle |
FILLET WELDS |
11-6. Poor Weld Bead Characteristics
1 Large Spatter Deposits
2 Rough, Uneven Bead
3 Slight Crater During Welding
4 Bad Overlap
5 Poor Penetration
1
2 3 4
5 |
11-7. Good Weld Bead Characteristics
1 Fine Spatter
2 Uniform Bead
3 Moderate Crater During
Welding
Weld a new bead or layer for each 1/8 in. (3.2 mm) thickness in metals being welded.
| 1 |
| 4 | No Overlap |
|
| 5 | Good Penetration into Base | |
|
|
| ||
|
|
|
| Metal |
2 | 3 | 4 | 5 |
|