PRODUCT
QUALITY
PROBLEMS
CONTINUED
Symptom | Possible cause Solution |
◆Cracks at cut site.
The extrudate is too cold. | If the extrudate is too cold, it |
| can fracture or whiten during |
| cutting. Raise the extrudate's |
| temperature. |
|
|
The blade speed is too | High blade speeds can cause |
high. | too much impact. Lower the |
| blade speed. |
|
|
The bushings are not pro- | Change the bushing design to |
viding enough support | make them more supportive. |
during cutting. |
|
|
|
The cutting blade is too | A blade that is too sharp can |
sharp. | fracture some materials, espe- |
| cially rigid PVC and nylons. |
| Slightly dull the blade. |
If using Nylon, it may be | If nylon is cooled too quickly, |
cooling too quickly. | its molecular structure may |
| become unstable, leading to |
| poor physical properties. Try |
| more gradual cooling. |
| TROUBLESHOOTING | UGE059/1003 |