CHAPTER 4
Table
Periods of appearance of dirt, blank spots on images
Problem location | Diameter | Period on |
| Phenomenon |
| ||
|
| Dirt on back |
| ||||
(mm) | image (mm) | Dirt | Blank spot | Poor fixing | |||
| of paper | ||||||
|
|
| |||||
Transfer charging roller | 17.15 | About 54 |
|
|
|
| |
|
|
|
|
|
|
| |
Upper fixing roller | 45 | About 141 |
|
|
|
| |
|
|
|
|
|
|
| |
Lower fixing roller | 32 | About 100 |
|
|
|
| |
|
|
|
|
|
|
| |
24 | About 75 |
|
|
|
| ||
|
|
|
|
|
|
| |
Feed roller | 24 | About 75 |
|
|
|
| |
|
|
|
|
|
|
| |
Separation roller | 24 | About 75 |
|
|
|
| |
Photosensitive drum | 30 | About 94 |
|
|
|
| |
|
|
|
|
|
|
| |
Developing cylinder | 20 | About 52 |
|
|
|
| |
|
|
|
|
|
|
| |
Primary charging roller | 14 | About 44 |
|
|
|
| |
|
|
|
|
|
|
|
4 - 13